How to Mix Perlite and Cement

Hunker may earn compensation through affiliate links in this story. Learn more about our affiliate and product review process here.
Create planters in all shapes and sizes using a concrete and perlite mix.
Image Credit: erperlstrom/iStock/Getty Images

Perlite concrete creates a lightweight concrete. It is not suitable for load-bearing applications, but commonly used for pool bases, roof decks and decorative purposes. Planters and statuary made with perlite concrete are porous and lightweight, providing ample drainage and making the objects easier to move. The ratio of cement to perlite depends on the insulation value and compressive strength you need -- more perlite in the mix increases insulation and decreases compressive strength. A 1-to-6 ratio of cement to perlite balances insulation and strength, and is suitable for most gardening applications. The order in which you add the ingredients is most important to avoid degrading the delicate perlite.

Advertisement

Step 1

Pour 1 cubic foot of dry cement in a wheelbarrow or concrete mixing machine. A 94-pound bag of cement is equivalent to 1 cubic foot. Increase or decrease the amount of cement based on your actual needs, but use 1 cubic foot as a reference point to achieve the proper ratio of ingredients.

Video of the Day

Step 2

Pour 13 gallons of water into the wheelbarrow or mixer. If you opt to make a smaller batch of perlite concrete, decrease the amount of water according to the decrease in cement. Add only 7 1/2 gallons of water, for example, if you use only half a bag of cement.

Advertisement

Step 3

Mix the cement and water until thoroughly combined. Mix with a garden hoe and shovel if you mix in a wheelbarrow, or turn the hand crank to tumble the ingredients inside a rotating concrete mixer. Scrape the sides of the wheelbarrow or mixer well to ensure all the dry cement is completely saturated.

Step 4

Pour 6 cubic feet of perlite into the wet cement mixture. Use only 3 cubic feet for half a 94-pound bag of cement, or 1 1/2 cubic feet when using one-fourth of the cement bag. Increase or decrease the amount of perlite as needed to achieve the desired insulation value and compressive strength. Perlite concrete mixed at a ratio of 1 part cement to 6 parts perlite has an insulation value, or "k" value, of 0.64 and a compressive strength of 125 to 200 pounds per square inch. At a ratio of 1 part cement to 4 parts perlite, you achieve a "k" value of 0.83 and compressive strength of 350 to 500 pounds per inch. At this ratio, you need only 10 gallons of water.

Advertisement

Step 5

Stir and turn the wet cement mix and perlite until the perlite is evenly distributed throughout the cement. Avoid overmixing the mixture or you can break down the structure of the perlite, which increases the density of the perlite cement.